SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D 792
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.10 %
0.10 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.40 %

@Temperature 23.0 °C
0.40 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Type I, 5 mm/min; ASTM D 638
55.0 MPa
7980 psi
5 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D 638
60.0 MPa
8700 psi
5 mm/min; ISO 527
Elongation at Break 110 %
110 %
Type I, 5 mm/min; ASTM D 638
110 %
110 %
5 mm/min; ISO 527
Elongation at Yield 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D 638
5.0 %
5.0 %
5 mm/min; ISO 527
Tensile Modulus 3.10 GPa
450 ksi
5 mm/min; ASTM D 638
3.10 GPa
450 ksi
1 mm/min; ISO 527
Flexural Yield Strength 95.0 MPa
13800 psi
1.3 mm/min, 50 mm span; ASTM D 790
95.0 MPa
13800 psi
2 mm/min; ISO 178
Flexural Modulus 3.00 GPa
435 ksi
1.3 mm/min, 50 mm span; ASTM D 790
3.00 GPa
435 ksi
2 mm/min; ISO 178
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
120 °C

@Thickness 3.20 mm
248 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 138 °C
280 °F
Rate B/50; ASTM D 1525
138 °C
280 °F
Rate B/50; ISO 306
140 °C
284 °F
Rate B/120; ISO 306
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2