Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East) High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 0.000 °C |
21.4 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® T50 BBS083 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® T65 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
ISO 180-A |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IL PA6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -40.0 °C |
21.4 ft-lb/in² @Temperature -40.0 °F |
ASTM D256 |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -40.0 °C |
21.4 ft-lb/in² @Temperature -40.0 °F |
ASTM D256 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacom™ ZG750 Polypropylene Copolymer Description: Hostacom™ ZG750 conventional melt flow, 1,700 MPa flexural modulus, 40% calcium carbonate-filled, utility grade polypropylene copolymer resin has a very good combination of strength, s.. |