Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DFP36 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone.
Mechanical Properties Metric English Comments
Tensile Strength at Break 98.0 MPa
14200 psi
5 mm/min; ISO 527
Elongation at Break 2.2 %
2.2 %
5 mm/min; ISO 527
Tensile Modulus 7.90 GPa
1150 ksi
1 mm/min; ISO 527
Flexural Yield Strength 127 MPa
18400 psi
2 mm/min; ISO 178
Flexural Modulus 5.20 GPa
754 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 51.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af