Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFP36 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP SFL36 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SFL36 is a compound based on PA 12 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | TMA |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM Test |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |