Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
ASTM D638
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched 17.08 J/cm
32.00 ft-lb/in
ASTM D4812