Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* JX91198 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 99.0 MPa
14400 psi
5 mm/min; ISO 527
Elongation at Break 1.6 %
1.6 %
5 mm/min; ISO 527
Flexural Strength 140 MPa
20300 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.34
0.34
ASTM D3702 Modified
Coefficient of Friction, Static 0.27
0.27
ASTM D3702 Modified
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257