Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* OCL36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Mechanical Properties Metric English Comments
Tensile Strength at Break 158 MPa
22900 psi
ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
ASTM D638
Flexural Modulus 23.16 GPa
3359 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 264 °C

@Thickness 3.20 mm
507 °F

@Thickness 0.126 in
unannealed; ASTM D648