Material Notes:
LNP* Lubricomp* RFN16 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
ASTM D638
Elongation at Break 2.9 %
2.9 %
ASTM D638
Tensile Modulus 9.56 GPa
1390 ksi
50 mm/min; ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 7.13 GPa
1030 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.04 J/cm
18.81 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: