Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP RN001 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RN001 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RN001 is a compound based on Nylon 66 resin containing MOS2.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
5 mm/min; ISO 527
Elongation at Break 6.6 %
6.6 %
5 mm/min; ISO 527
Elongation at Yield 5.4 %
5.4 %
5 mm/min; ISO 527
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
Flexural Strength 91.0 MPa
13200 psi
2 mm/min; ISO 178
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: