SABIC Innovative Plastics LNP STAT-KON DE0069F PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DE0069F PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* DE0069F is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, , Flame Retardant.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
ASTM D638
Tensile Modulus 17.23 GPa
2499 ksi
50 mm/min; ASTM D638
Flexural Strength 199 MPa
28900 psi
ASTM D790
Flexural Modulus 16.54 GPa
2399 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C

@Thickness 3.20 mm
286 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 6.0 ohm
1.0 - 6.0 ohm
ASTM D257