Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Bearing Grade, Electrically Conductive, Wear R.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 5.0 ohm | 1.0 - 5.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific) LNP* Stat-kon* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific) LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 05004 FR Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific) LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, .. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific) LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON SD000 PA12 LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | IEC 60093 |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Flame Retardant, Wear Resi.. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 (Asia Pacific) LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabil.. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | |
A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | IEC 60093 |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend) |