Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Glass Fiber Reinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* KF004A is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Time 86400 sec
0.0060 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 99.0 MPa
14400 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Strength 144 MPa
20900 psi
ASTM D790
Flexural Modulus 7.10 GPa
1030 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Users viewing this material also viewed the following: