Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 227 MPa
32900 psi
5 mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
Flexural Strength 321 MPa
46600 psi
2 mm/min; ISO 178
Flexural Modulus 19.6 GPa
2840 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Electrical Properties Metric English Comments
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257