Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | Crystalline; ISO 1183 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Mitsubishi Xantar® SF 2230 Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Electrablend® POM CF15 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerAppearance: Natural ColorInformation provided by TP Composites, Inc... |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF40 RM HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer Features: Heat Stabilized and Low Moisture AbsorptionAppearanc.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PC GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0142 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific) LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 329 Polyester Film, 300 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex.. |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 011 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 86/R Flexible PVC, Sheathing Hydrocarbon resistant |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 74/R Flexible PVC, Flame Retardant Sheathing Mineral oil resistent |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB7 GR15 NL RT PBT, 15% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade Information provided by Eurotec® |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Celanese Hostaform® LX90Z XAP2 ™ POM, UV Resistant Preliminary Data SheetDrying is required for this material to prevent poor appearance and performance of the part.Information provided by Celanese Corporation. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Celanese Thermx® CG053 PCT, 28% Mineral / Glass Reinforced Thermx® CG053 is a 28% glass/mineral reinforced polycyclohexylenedimethylene terephthalate resin.28% glass/mineral reinforcedInformation provided by Celanese |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® P1430 Polycarbonate, 30% Glass Reinforced A 30% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1433 with UV stabilizer.Data provided by the manufacturer |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | (Dry) |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Celanese Hostaform® LX90Z XAP² ™ POM, UV Resistant
(Unverified Data**) Preliminary Data SheetLow emission, UV resistant grade, Metallic colorsInformation provided by Celanese |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |