Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PC006 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PC006 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* PC006 is a compound based on Nylon 6 resin containing Carbon Fiber.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 182 MPa
26400 psi
5 mm/min; ISO 527
Elongation at Break 2.2 %
2.2 %
5 mm/min; ISO 527
Flexural Strength 275 MPa
39900 psi
2 mm/min; ISO 178
Flexural Modulus 15.4 GPa
2230 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
Electrical Properties Metric English Comments
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257