Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PF00C is a compound based on Nylon 6 resin containing 60% Glass Fiber.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Tensile Modulus 22.38 GPa
3246 ksi
50 mm/min; ASTM D638
Flexural Strength 365 MPa
52900 psi
ASTM D790
Flexural Modulus 19.38 GPa
2811 ksi
ASTM D790
Izod Impact, Notched 1.70 J/cm
3.18 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.29 J/cm
23.02 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C

@Thickness 3.20 mm
410 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: