Polymer Property : Izod Impact, Unnotched = 12.29 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.29 J/cm
23.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Asia Pacific)
LNP* Thermocomp* PF00C is a compound based on Nylon 6 resin containing Glass Fiber.
Izod Impact, Unnotched 12.29 J/cm
23.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6
LNP* THERMOCOMP* PF00C is a compound based on Nylon 6 resin containing 60% Glass Fiber.