Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 113 MPa
16400 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 6.39 GPa
927 ksi
50 mm/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 6.26 GPa
908 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.48 J/cm
8.39 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 222 °C

@Thickness 3.20 mm
432 °F

@Thickness 0.126 in
unannealed; ASTM D648