SABIC Innovative Plastics LNP THERMOTUF IX02582 PA 6/12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF IX02582 PA 6/12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Moisture Absorption 0.250 %
0.250 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 2.08 J/cm
3.90 ft-lb/in
ASTM D256