Material Notes:
LNP THERMOTUF* RF002I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 107 MPa
15500 psi
ASTM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Tensile Modulus 4.82 GPa
699 ksi
50 mm/min; ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 4.34 GPa
629 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C

@Thickness 3.20 mm
399 °F

@Thickness 0.126 in
unannealed; ASTM D648