SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 6.00 g/cc
0.217 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D 638
Elongation at Yield 3.5 %
3.5 %
ASTM D 638
Tensile Modulus 0.710 GPa
103 ksi
50 mm/min; ASTM D 638
Flexural Strength 68.0 MPa
9860 psi
ASTM D 790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D 790
Izod Impact, Notched 0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763