Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.00 g/cc | 0.217 lb/in³ | |
NanoScale NanoActive® Cerium Oxide NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials F-200-P Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-10All information provided by Pacific Sintered Metals. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals Copper Steel FC-221-P Powdered Metal Medium strength mechanical components Equivalent MPIF Specification: FC-0205-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-200-P Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-10Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | |
Piezo Kinetics PKI 100 Lead Metaniobate Piezoelectric Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | |
MarkeTech Ceraflex 3Y Thin Zirconia Ceramic, Yttria Stabilized Data provided by the supplier, MarkeTech International.3 mole% Y2O3 (5.35 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are .. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | |
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ) Brand 868 features: High density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal c.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | |
MMCC Cu/Al2O3 Particulate Copper Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 (Asia Pacific) LNP* THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific) LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | |
China Tungsten YT772-1 Titanium Carbide and Nitride Based Carbides Of wear resistance near ceramics good thermo-stability and less toughness, for continuous finishing of carbon steel, alloy steel, stainless steel, tol steel and chilled steel to very high fineness.I.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |
|||
Density | 6.00 g/cc | 0.217 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPU 0600 Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |