Material Notes:
LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ISO 294
0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ISO 294
0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 232 MPa
33600 psi
ISO 527
261 MPa
37900 psi
ASTM D 638
Elongation at Break 1.0 %
1.0 %
ASTM D 638
1.3 %
1.3 %
ISO 527
Tensile Modulus 33.78 GPa
4899 ksi
50 mm/min; ASTM D 638
35.53 GPa
5153 ksi
1 mm/min; ISO 527
Flexural Strength 425 MPa
61600 psi
ISO 178
441 MPa
64000 psi
ASTM D 790
Flexural Modulus 26.59 GPa
3857 ksi
ISO 178
26.82 GPa
3890 ksi
ASTM D 790
Izod Impact, Notched 0.580 J/cm

@Temperature 23.0 °C
1.09 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.20 J/cm

@Temperature 23.0 °C
5.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 5.00 J
3.69 ft-lb
Multiaxial Impact; ISO 6603
7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 250 °C
>= 482 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
>= 248 °C

@Thickness 3.20 mm
>= 478 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D 257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D 257
Users viewing this material also viewed the following: