Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific) LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 (Asia Pacific) LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized... |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific) LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX96717C PC LNP STAT-KON* DX96717C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific) LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Europe-Africa-Middle East) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA LNP THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0080 cm/cm @Time 86400 sec |
0.0070 - 0.0080 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12 LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 3.00 mm |
0.0070 in/in @Thickness 0.118 in |
Mold 80°C; ISO 294-4 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
Mold 80°C; ISO 294-4 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 3.00 mm |
0.0070 in/in @Thickness 0.118 in |
Mold 80°C; ISO 294-4 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |