Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RX04493D PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RX04493D PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* RX04493D is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this grade is: Structural.
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 270 MPa
39200 psi
ASTM D638
Flexural Modulus 17.16 GPa
2489 ksi
ASTM D790
Izod Impact, Notched 4.80 J/cm
8.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C

@Thickness 3.20 mm
486 °F

@Thickness 0.126 in
unannealed; ASTM D648