SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS Auto Exterior Grade
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
SABIC - Japan Method
Elongation at Break 50 %
50 %
SABIC - Japan Method
Flexural Strength 78.0 MPa
11300 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 55.0 - 75.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
30.6 - 41.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
unannealed; ASTM D648