SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl PPX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PP blend. Suitable for painted exterior automotive applications.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Melt Index of Compound 12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ISO 2039-2
Tensile Strength at Break 34.0 MPa
4930 psi
50 mm/min; ISO 527
Tensile Strength, Yield 36.0 MPa
5220 psi
50 mm/min; ISO 527
Elongation at Break 110 %
110 %
50 mm/min; ISO 527
Elongation at Yield 5.5 %
5.5 %
50 mm/min; ISO 527
Tensile Modulus 1.70 GPa
247 ksi
1 mm/min; ISO 527
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 39.0 kJ/m²
18.6 ft-lb/in²
80*10*4; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 3.80 J/cm²
18.1 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 78.0 °C
172 °F
Rate B/50; ISO 306
83.0 °C
181 °F
Rate B/120; ISO 306