SABIC Innovative Plastics NORYL PX2630 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX2630 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+HIPS Unfilled high Impact
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 250 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
SABIC - Japan Method
Elongation at Break 42 %
42 %
SABIC - Japan Method
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.09 GPa
303 ksi
ASTM D790
Izod Impact, Notched 3.30 J/cm
6.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648