Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® VAC3003 PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D 792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.017 - 0.023 cm/cm

@Thickness 3.20 mm
0.017 - 0.023 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D 785
Tensile Strength, Yield 50.0 MPa
7250 psi
SABIC - Japan Method
Elongation at Break 30 %
30 %
SABIC - Japan Method
Flexural Strength 79.0 MPa
11500 psi
ASTM D 790
Flexural Modulus 2.35 GPa
341 ksi
ASTM D 790
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature -30.0 - 30.0 °C
72.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C

@Thickness 3.20 mm
131 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94