S&E Specialty Polymers G-4275E

Category Polymer , Thermoplastic
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers G-4275E.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: General-purpose extrusion material designed for profile extrusion applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.45 g/cc
1.39 - 1.45 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 80
75 - 80
ASTM D2240
Tensile Strength 11.6 MPa
1680 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D2863