S&E Specialty Polymers G-4785E PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers G-4785E PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Flexible, PVC material designed for general-purpose extrusion applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.50 g/cc
1.44 - 1.50 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 90
85 - 90
ASTM D2240
Tensile Strength 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D412
100% Modulus 0.0103 GPa
1.50 ksi
ASTM D412