Material Notes:
Application: Thermoplastic polyolefin material is designed for automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or paintable versionInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ISO 1183
Melt Flow 15.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 18.6 MPa
2700 psi
ISO 527
Flexural Modulus 1.465 GPa
212.5 ksi
ISO 178
Impact Test 18.0 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
20.0 J

@Temperature 0.000 °C
14.8 ft-lb

@Temperature 32.0 °F
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763