Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFlex™ GA-5330D PVC/PU Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFlex™ GA-5330D PVC/PU Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: 105°C, matte finish, flame retardant PVC/PU jacketing material designed for retractile cord applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80.0

@Time 15.0 sec
80.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 19.0 MPa
2760 psi
ASTM D412
15.2 MPa

@Temperature 136 °C,
Time 605000 sec
2200 psi

@Temperature 277 °F,
Time 168 hour
Air Oven Aged
Elongation at Break 400 %
400 %
ASTM D412
220 %

@Treatment Temp. 136 °C,
Time 605000 sec
220 %

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven Aged
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Oxygen Index 25.0 %
25.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 171 - 179 °C
340 - 355 °F
Suggested Extusion Stock
Users viewing this material also viewed the following: