Material Notes:
Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90.0

@Time 15.0 sec
90.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 18.3 MPa
2650 psi
ASTM D412
19.032 MPa

@Temperature 100 °C,
Time 864000 sec
2760.4 psi

@Temperature 212 °F,
Time 240 hour
Aged
Elongation at Break 300 %
300 %
ASTM D412
255 %

@Treatment Temp. 100 °C,
Time 864000 sec
255 %

@Treatment Temp. 212 °F,
Time 240 hour
Aged
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -26.0 °C
-14.8 °F
ASTM D746
Oxygen Index 27.0 %
27.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 177 - 182 °C
350 - 360 °F