Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 1725-xx13FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon® W3201 is UL recognized for UL 94 V0 per QMFZ2, and is suitable for injection molding. This product meets UL 105°C, AWM, and Mil-W-76 80°C insulation.NOTE: Typical Properties of Molded Slab .. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-3174D PVC Compound Application: RoHS compliant, 60°C , general purpose PVC based compound suitable for extrusion applications.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-7056-1002 PVC Compound Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 90253 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 2085-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 3085-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 3310-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 3310-80NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Food Service Applications; Medical/Healthcare Applications; Tubing Processing Forms: Extrusion Forms: PelletsInformation Provided by Tek.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 3600-90NT Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 02-A0310A-107 Polyvinyl Chloride, Semi-Rigid Notes: 80°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: GPTAgency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor .. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | |
Daikin DAI-EL G-555 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | |
Daikin DAI-EL G-901 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance.Information provided by Daikin Industries. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | |
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | |
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4725P Heat Resistant Molding FormulationNordel® IP 4725P |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7816 Flexible PVC, Injection Molding for Footwear Soles for mild climates |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Colorite Polymers CS8036CS Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 80 Flexible PVC, Extrusion Modified with Rubber Profiles modified with rubber |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D-746 |
Axiall 13871 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D-746 |
Axiall 13872 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75°C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in .. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D-746 |
Axiall 14840 Wire & Cable Flexible PVC General purpose jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Teknor Apex APEX® 3210-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W2413 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -26.0 °C | -14.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8020 Flexible PVC, Lead Free Covering steel sheaths |