S&E Specialty Polymers XP23-566-1 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers XP23-566-1 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PVC weatherable, integral colored, filledApplication: Low gloss lift gate molding compound which meets Chrysler MSDC 543.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity <= 1.30 g/cc
<= 1.30 g/cc
ASTM D792, A
Mechanical Properties Metric English Comments
Hardness, Shore D 34 - 40

@Time 15.0 sec
34 - 40

@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 15.0 MPa
>= 2180 psi
Type IV, 500mm/min; ASTM D638
Elongation at Break >= 200 %
>= 200 %
Type IV, 500mm/min; ASTM D638
Tear Strength >= 45.0 kN/m
>= 257 pli
Method B; ISO 34
Descriptive Properties Value Comments
Accelerated Weathering <3.0 DE
after 2000 kj/m<sup>2</sup>, SAEJ2527
Cold Flex -30°C
GM9503P