SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP
Manufacturer SK Chemicals
Trade Name SKYPEL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Tensile Strength, Yield 7.26 MPa

@Strain 5.00 %
1050 psi

@Strain 5.00 %
ASTM D638
11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 880 %
880 %
ASTM D638
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Tear Strength 165 kN/m
941 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648