Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Water Absorption 2.9 %
2.9 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
ASTM D2240
Tensile Strength, Ultimate 11.8 MPa
1710 psi
ASTM D638
Tensile Strength, Yield 1.47 MPa

@Strain 5.00 %
213 psi

@Strain 5.00 %
ASTM D638
2.94 MPa

@Strain 10.0 %
427 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 370 %
370 %
ASTM D638
Flexural Modulus 0.0333 GPa
4.84 ksi
ASTM D790
Resilience 66
66
ASTM D2632
Izod Impact, Notched 2.26 J/cm
4.22 ft-lb/in
ASTM D256
Tear Strength 55.0 kN/m
314 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 189 °C
372 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °C
126 °F
ASTM D648