SK Chemicals SKYTHANE® 850A T series Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® 850A T series Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
ASTM D2240
Hardness, Shore D 12
12
ASTM D2240
Tensile Strength, Ultimate 11.8 MPa
1710 psi
ASTM D412
Tensile Strength, Yield 1.47 MPa

@Strain 100 %
213 psi

@Strain 100 %
ASTM D412
3.92 MPa

@Strain 300 %
569 psi

@Strain 300 %
ASTM D412
Elongation at Break 770 %
770 %
ASTM D412
Resilience 60
60
by vertical rebound; ASTM D2632
Tear Strength 49.0 kN/m
280 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525