Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 49.0 kN/m | 280 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8502 CLASSY GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 15%. Multi-Flex TPE contains Krato.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ASTM D624 |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-2175 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tear Strength | 49.0 kN/m | 280 pli | 49 kN/m at 23°C. Value at 100°C is 23 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tear Strength | 49.1 kN/m | 280 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ASTM D790 |
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tear Strength | 49.0 kN/m | 280 pli | B-type, Vulcanized |
KKPC KOSYN 1502G Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | B-type, Vulcanized |
KKPC KOSYN 1502LL Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | B-type, Vulcanized |
KKPC KOSYN 1502NF Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | B-type, Vulcanized |
KKPC KOSYN 1507L Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | Die C; ASTM D624 |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ASTM D624 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Tear Strength | 49.0 kN/m | 280 pli | B-type, Vulcanized |
KKPC KOSYN 1507 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ASTM D624 |
Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Moldability, GoodPaintable Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsInforma.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 49.0 kN/m | 280 pli | ASTM D624 |
SK Chemicals SKYTHANE® UB410 Powder Coating Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP 1093L Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | ASTM D624 |
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | 500 mm/min; ASTM D 624 |
Zylog Neoplast® 180 C Thermoplastic Vulcanizate Neoplast 180 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV S.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | 500 mm/min; ASTM D 624 |
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tear Strength | 49.0 kN/m | 280 pli | ISO 34B |
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | Die B; Silicone Property; ASTM D624 |
Arlon 99020N015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data represents typical values for the pro.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ISO 34-1 |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | ISO 34-1 |
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 49.1 kN/m | 280 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 49.0 kN/m | 280 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |