Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloyClips: Stainless steelThreaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 18.8 daN
11.0 mm, 45° down and out
32.0 daN
8.8 mm, down
33.5 daN
4.1 mm, up
34.5 daN
8.2 mm, up and down
34.5 daN
8.7 mm, left and right
F, Max Static 10.0 daN
1.8 mm, down
10.0 daN
1.3 mm, up
10.0 daN
2.6 mm, 45° down and out
5.0 daN
2.0 mm, up and down
5.0 daN
2.2 mm, left and right
Transmissibility at resonance 3