Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 20.0 - 300 °C | 68.0 - 572 °F | Average value: 121 °C Grade Count:59 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Maximum Service Temperature, Air | 120 - 300 °C | 248 - 572 °F | Average value: 176 °C Grade Count:9 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Maximum Service Temperature, Air | 260 - 300 °C | 500 - 572 °F | Average value: 264 °C Grade Count:17 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2513S-10-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2513S-30-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2514S-10-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2514S-40-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2515S-10-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2515S-20-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2516S-30-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2516S-40-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2518S-20-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2518S-30-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2518S-60-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2519S-30-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2519S-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2521S-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2521S-60-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 25235-30-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2524S-10-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2524S-30-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2526S-20-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 150 - 300 °C @Pressure 0.000 - 5.00 MPa |
302 - 572 °F @Pressure 0.000 - 725 psi |
Recommended Application Range |
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data.. |
|||
Maximum Service Temperature, Air | 150 - 300 °C @Pressure 0.000 - 5.00 MPa |
302 - 572 °F @Pressure 0.000 - 725 psi |
Recommended Application Range |
Arlon UltraPad™ 51073R031D Silicone-Based Press Pad UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre.. |
|||
Maximum Service Temperature, Air | 100 - 300 °C @Pressure 0.000 - 10.0 MPa |
212 - 572 °F @Pressure 0.000 - 1450 psi |
|
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
Maximum Service Temperature, Air | 98.0 - 300 °C | 208 - 572 °F | Average value: 227 °C Grade Count:6 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Maximum Service Temperature, Air | 107 - 300 °C | 225 - 572 °F | Average value: 185 °C Grade Count:3 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 25235-10-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 25235-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2524S-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro.. |