Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SMAC CABLE® 2521S-10-08 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name CABLE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC CABLE® 2521S-10-08 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloy Screws: Inox A2Threaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 2430 daN
20.0 mm, up
530.0 daN
55.0 mm, 45° down and out
760.0 daN
35.0 mm, left and right
820.0 daN
28.4 mm, up and down
880.0 daN
37.0 mm, down
F, Max Static 148.0 daN
9.1 mm, up and down
148.0 daN
13.0 mm, left and right
220.0 daN
11.5 mm, 45° down and out
295.0 daN
7.0 mm, down
295.0 daN
5.0 mm, up
Transmissibility at resonance 3