Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloy Screws: Inox A2Threaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 1010 daN
103.0 mm, up and down
3120 daN
62.0 mm, up
585.0 daN
125.0 mm, 45° down and out
935.0 daN
85.0 mm, down
965 daN
95.0 mm, left and right
F, Max Static 155.0 daN
27.1 mm, up and down
155.0 daN
29.0 mm, left and right
235.0 daN
28.0 mm, 45° down and out
310.0 daN
15.5 mm, down
310.0 daN
13.5 mm, up
Transmissibility at resonance 3
Users viewing this material also viewed the following: