SMAC SMACMOUNT® 2112S 01 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 2112S 01 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCountersunk for lowest installed heightCan be pre-loaded to vary natural frequencyAxial to radial stiffness ratio of approx. 1:1Information provided by SMAC MontBlac Groupe Technologies
Descriptive Properties Value Comments
Load .5 kg
40 Hz, Natural frequency
<2 kg
10 kg
2 mm, Static Deflection
2.1 kg
23 Hz, Natural frequency
20 kg
3 mm, Static Deflection
5 kg
1 mm, Static Deflection