Material Notes:
Specifications - Shock & vibration insulation for:Airborne components and electronic packagesMissile systems and electronicsAirborne avionics unitsGyro, optic, & laser components and assembliesAdvantages:Low profileNear 1 to 1 axial to radial springrate ratioDouble the stiffness and countersink using 2 mounts back to backInformation provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
Descriptive Properties Value Comments
Axial/Radial frequency ratio 1/1 approx.
Frequency 16 - 27 Hz
Materials SMACSIL®
Maximum axial deflection 5.1 mm
Maximum input at resonance (DA) 0.9 mm
Metal parts Alu alloy
chromate treated per MIL-C-5541 cl. 1A
Transmissibility at resonance 8
Weight 9.6 g