Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 51.7 - 150 °C | 125 - 302 °F | Average value: 109 °C Grade Count:59 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 80.0 - 150 °C | 176 - 302 °F | Average value: 131 °C Grade Count:8 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Maximum Service Temperature, Air | 127 - 150 °C | 260 - 302 °F | Average value: 140 °C Grade Count:34 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 75.0 - 150 °C | 167 - 302 °F | Average value: 113 °C Grade Count:3 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Maximum Service Temperature, Air | 90.0 - 150 °C | 194 - 302 °F | Average value: 118 °C Grade Count:8 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 90.0 - 150 °C | 194 - 302 °F | Average value: 123 °C Grade Count:10 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | SMACSIL® |
SMAC SMACDISK® 1114S Damping Material Specifications - Shock & vibration insulation for:Hard diskLow frequency dampingVehicular electronicsRequiring vibration isolationInformation provided by SMAC MontBlac Groupe Technologies |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | SMACSIL® |
SMAC SMACMOUNT® 1195S Damping Material Specifications - Shock & vibration insulation for:Embedded electronicTrays & racks systemsAdvantages:No special tools requiredHigh damping isolatorsSmall SizeInformation provided by SMAC MontBlac Gr.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | SMACSIL® |
SMAC SMACMOUNT® 2528S Damping Material Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCou.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | |
SMAC SMACMOUNT® 2112S Damping Material Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCou.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | |
SMAC SMACMOUNT® 2132S Damping Material Specifications - Shock & vibration insulation for:Airborne components and electronic packagesMissile systems and electronicsAirborne avionics unitsGyro, optic, & laser components and assembliesAdvan.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | |
SMAC SMACMOUNT® 2150S Damping Material Specifications - Shock & vibration insulation for:Electronic components and subassemblies (Disk drive, Guidance system, radar…)High frequency vibration isolationStructural element vibration bre.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | |
SMAC SMACMOUNT® 2151S Damping Material Specifications - Shock & vibration insulation for:Electronic components and subassemblies (Disk drive, Guidance system, radar…)High frequency vibration isolationStructural element vibration bre.. |
|||
Maximum Service Temperature, Air | -55.0 - 150 °C | -67.0 - 302 °F | |
SMAC SMACMOUNT® 2527S Damping Material Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesAirborn electronicsAdvantages:Light weightSave spaceDouble the stiffness and countersink using 2 mounts .. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | |
Goodfellow E-glass/Epoxy Composite Boro-silicate glass/EpoxyInformation provided by Goodfellow. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Maximum Service Temperature, Air | 100 - 150 °C | 212 - 302 °F | Average value: 111 °C Grade Count:16 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | Average value: 140 °C Grade Count:12 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | Average value: 140 °C Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | Average value: 140 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |