SMAC SMACMOUNT® 2151S Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 2151S Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specifications - Shock & vibration insulation for:Electronic components and subassemblies (Disk drive, Guidance system, radar…)High frequency vibration isolationStructural element vibration breakMissile and avionic modulesAdvantages :Bushing style mountRequires minimal space for installationCan be preloaded to adjust and tune performanceWasher creates snubbing feature on bottom side of mountInformation provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
Descriptive Properties Value Comments
Axial/Radial frequency ratio 1/1 approx.
Frequency 185 Hz
01
185-230 Hz
210 Hz
02
230 Hz
03
Load 2.3 kg
01
2.3 kg
02
2.3 kg
03
Materials SMACSIL®
Maximum axial deflection 0.4 mm
Maximum input at resonance (DA) 3 g
Metal parts Stainless steel
Overall size 17.5 x 10 mm
Transmissibility at resonance <3.5
SMACSIL®
Weight 5.7 g