SPS Guang Zhou POLLITEâ„¢ 1001(+) Flame-retarded Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer SPS Guang Zhou
Trade Name POLLITE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou POLLITEâ„¢ 1001(+) Flame-retarded Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: Good flame retardance, high notched impact strength, high heat resistanceApplications: Computer, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
Flexural Modulus 2.30 GPa
334 ksi
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 V-0
V-0