Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 85FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD123R PC (Europe-Africa-Middle East) LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD2034 PC (Europe-Africa-Middle East) LEXAN FXD2034 is a translucent medium viscosity flame retardant grade for light diffusion applications. The material is UV-stabilized. Can meet I2 rating according NF F16101.This data was supplied b.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE161R PC (Europe-Africa-Middle East) LEXAN FXE161R is a transparent/translucent medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE161R contains a release agent to ens.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM123R PC (Europe-Africa-Middle East) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East) IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® PK2870 PC LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® VR1820 PC (Europe-Africa-Middle East) VR1820 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East) Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability. |
|||
Flexural Modulus | 2.30 - 9.74 GPa | 334 - 1410 ksi | Average value: 6.64 GPa Grade Count:10 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East) Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM921A PC (Europe-Africa-Middle East) LEXAN FXM921A is a transparent/translucent, medium viscosity, flame retardant grade with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2mm/min; ASTM D790 |
Kingfa JH950-402 Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2mm/min; ASTM D790 |
Kingfa MAC-601 AC PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2mm/min; ASTM D790 |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East) Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D 790 |
Cossa Polimeri ESTABLEND 4500 T V0 Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE free, with halogens, high impact resistance, high thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D790, ISO 178 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D790 |
Ashley Polymers Ashlene® PC/ABS Alloy 306 General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
Polyram RamOfin PPC350M6 Polypropylene, 30% Mineral Filled 30% Mineral filled, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |